Anti-corrosion finish for copper intercooler?

Started by Dakin Engineering, January 01, 2008, 06:12:24 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

panic

IIRC a sacrificial metal will help in proportion to its relative position on the scale of activity. Copper is relatively inert, so anything higher (magnesium and aluminum best in that order) will work. There are more active metals (lithium, barium, potassium, sodium, calcium) but they react violently with water.

Stainless1

What does the 3-5 degree colder salt ice water do over non-corrosive plain ice water?  Did your experiments include Water Wetter or any of the equivalent non-corrosive products?  50/50 antifreeze?  Just thoughts... It is always better to keep it simple, even if the supply of salt seems unlimited....  8-)
Stainless
Red Hat 228.039, 2001, 65ci, Bockscar Lakester #1000 with a little N2O

Dakin Engineering

Stainless,
  Ya got me there. My testing showed no appricable gain with the brine solution.
But, since Salt gets everywhere, well....
  It'll look much nicer inside the SS box, anyway.

Sam
Turbo Sportsters since '97